Meaning
Hazardous conditions occur when an increase in temperature changes the environment in a way that causes a further increase in temperature, often leading to a destructive result. Lithium ion batteries are susceptible to thermal runaway if internal defects or external damage initiate an exothermic reaction that exceeds the cooling capacity of the system. Such a process is self sustaining once it reaches a critical temperature threshold.
Chemical Initiation
Decomposition of the solid electrolyte interface layer begins the sequence of events that leads to total failure. When this protective layer breaks down, the anode reacts directly with the electrolyte, releasing heat and gas. If the heat generation exceeds the rate of heat dissipation, the separator melts and a short circuit occurs.
Propagation Velocity
Energy release happens with extreme speed as the reaction spreads from a single cell to neighboring units in a battery pack. In a large scale storage system, thermal runaway can move through the entire array in a matter of minutes if fire suppression systems fail to intervene. The high density of energy stored in modern batteries makes this transition difficult to stop once the chemical breakdown is widespread.
Mitigation Strategy
Safety protocols involve the use of flame retardant additives and durable cooling channels to prevent the initial temperature spike. Sensors detect the venting of gas or a rapid change in voltage that precedes thermal runaway in an operational battery. Passive barriers between cells are often installed to contain the heat and prevent it from affecting the rest of the module.
These barriers are constructed from materials with high thermal resistance and low flammability.