Meaning
Quality control outcome where a metal part fails to meet structural or dimensional specifications after a compression process. A forging rejection occurs when internal or external defects make the component unsuitable for its intended engineering application. This event marks a loss of the value added during heating and shaping, often necessitating the scrapping of the material.
Defect Origin
Common causes for such failures include laps, seams, cold shuts or internal cracks that weaken the metal matrix. During a thorough inspection, a forging rejection may be triggered by visual flaws or by more advanced non-destructive testing such as ultrasonic or dye penetrant examination. These defects frequently originate from improper temperature control or incorrect lubricant application during the press cycle.
Detailed logging of these occurrences is required to maintain the aerospace or medical certification of a plant.
Inspection Criteria
Corrective actions are sometimes possible if the flaw is purely superficial and the part remains above the minimum required dimensions. If the forging rejection results from a systemic issue in the die design or the material flow, the entire production batch may need to be quarantined for re-evaluation. Documenting these failures allows the engineering team to adjust the grain flow or the forging pressure in future runs.
Financial Consequence
Economic losses from these events extend beyond the cost of the raw metal to include the energy used in the furnaces and the labour of the operators. Frequent forging rejection rates can destabilise a supply chain by causing delays in the delivery of critical components to the final assembly plant.