Meaning
Multilayer polymer films and polymer blends can experience chemical reactions at their contact boundaries during high-temperature co-extrusion or blending. The development of a transesterification interphase involves the exchange of ester groups between different polyester chains at the melt boundary, creating a copolymer layer that links the distinct phases. This reaction increases the interfacial adhesion between the otherwise incompatible polymer layers, reducing the risk of delamination.
However, excessive reaction can alter the mechanical properties of the blend.
Chemical Mechanism
The reaction occurs through direct ester-ester exchange or alcoholysis between the chain ends of the polyesters. Formation of the transesterification interphase is accelerated by high melt temperatures and the presence of residual catalyst from the polymerization process. If the temperature is too low, the diffusion rate is insufficient to allow the chains to interact.
The reaction rate must be controlled to prevent complete randomized blending of the polymers.
Adhesion Control
The thickness of the transesterification interphase determines the mechanical strength of the multi-layer film. If the reaction is too limited, the layers will easily peel apart under low mechanical load. To optimize adhesion, the temperature and residence time in the extruder must be carefully balanced.
Adding specific catalysts or inhibitors allows manufacturers to control the rate of the transesterification reaction and achieve the desired interphase thickness.
Processing Boundary
If the processing temperature exceeds the degradation point of either polyester, thermal degradation will override the beneficial transesterification reaction. This degradation results in a weak interphase that brittlely cracks under stress, ruining the product’s performance.