Meaning
Chemical breakdown of polymer chains through the reaction with water molecules targets sensitive functional groups such as esters, amides, or anhydrides in the backbone. Hydrolytic scission occurs most frequently in condensation polymers where the presence of moisture at elevated temperatures reverses the polymerization reaction. This process leads to a significant decrease in molecular weight and a corresponding loss of impact strength.
Moisture Sensitivity
High levels of humidity combined with heat provide the energy required for water molecules to penetrate the amorphous regions and attack the chemical bonds. For the moisture sensitivity of hydrolytic scission, the rate of degradation is proportional to the concentration of water within the material. Polyamides and polyesters are particularly vulnerable if they are not thoroughly dried before processing.
Chain Fragmentation
Extensive reaction between the water and the polymer backbone results in the breaking of the long chains into shorter fragments. These smaller molecules increase the mobility of the remaining structure, which initially leads to an increase in crystallinity but eventually causes the material to become brittle. Surface cracks often appear as the fragmentation continues.
Acidic Catalysis
Acidic or basic impurities in the resin or the environment can significantly increase the speed of the reaction. During hydrolytic scission, the presence of carboxyl end groups created by the initial breaks can act as a catalyst for further degradation. This autocatalytic behavior means the rate of failure increases over time.